In resistance brazing, the source of power supply is Step-down transformer.
In resistance brazing, the source of power supply is Step-down transformer.
Spelter is a brazing alloy consisting 50% copper and 50% zinc.
It is impossible to braze aluminium with normal brass brazing rods because, aluminium has a too low melting point and would melt before brass.
Melting Temperature of Brass normally 900 Degree Centigrade to 940 Degree Centigrade.
Melting Temperature of aluminium normally around 660.3 Degree Centigrade.
Emery cloth is used as abrasive materials to clean the steel before brazing.